Material-technical base

Hammers Schmidt 20

Designed for non-destructive testing of mortar strength in stone masonry. The method consists in measuring the height of the rebound of the striker, which falls on the investigated surface, having a certain energy. The height of the rebound is converted into strength (MPa) on the grading curves.

  • Impact energy, J – 196
  • Measurement range, MPa 1-25
  • Measurement mistake, % ±10
  • The thickness of the sample material, mm – 30